Siliciumstaal spoel amorf magnetische kern met hoge verzadigingsmagnetische inductie, laag magnetisch verlies en goede frequentieprestaties
Silicon Steel Coil Product Performance High saturation magnetic induction Bs Low magnetic loss compared to other materials Excellent frequency and temperature performance, suitable for 3000KHz applications High DC bias characteristics Low magnetic leakage rate Lighter weight and smaller size compared to alternative materials Technical Specifications Density 7.3 g/cm³ Curie temperature Tc = 410°C Essence temperature Tx = 530°C Saturation Bs = 1.56T Resistivity ρ = 130 Ω-cm