"low magnetic loss amorphous magnetic core"
-
Silicon Steel Coil Amorphous Magnetic Core with High Saturation Magnetic Induction Low Magnetic Loss and Good Frequency Performance
Silicon Steel Coil Product Performance High saturation magnetic induction Bs Low magnetic loss compared to other materials Excellent frequency and temperature performance, suitable for 3000KHz applications High DC bias characteristics Low magnetic leakage rate Lighter weight and smaller size compared to alternative materials Technical Specifications Density 7.3 g/cm Curie temperature Tc = 410C Essence temperature Tx = 530C Saturation Bs = 1.56T Resistivity = 130 -cm